Produktbild BHP Polyester

Polyester

Delivered from 1kg to 225kg

Thixotropic polyester resin for reinforcement with glass fibre mat.

Instructions

Do not work in direct sunlight. Ambient temperature and the temperature of the object should be between 18-25°C. Add approx. 2% hardener just before application and mix well. Spread the resin thickly and apply the glass fibre mat. Press down the mat with a brush or aluminium roller until the mat is thoroughly saturated and there are no more air bubbles. Repeat until desired thickness is achieved.

Can be sanded in 3 hours
Cleaning Acetone